The nature of iron-oxygen vacancy defect centers in PbTiO3
Mestric, H. · Eichel, R. -A. · Kloss, T. · Dinse, K. -P. · Laubach, So. · Laubach, St. · Schmidt, P. C. · Schoenau, K. A. · Knapp, M. · Ehrenberg, H.
Original · EN
The iron(III) center in ferroelectric PbTiO3 together with an oxygen vacancy forms a charged defect associate, oriented along the crystallographic c-axis. Its microscopic structure has been analyzed in detail comparing results from a semi-empirical Newman superposition model analysis based on finestructure data and from calculations using density functional theory. Both methods give evidence for a substitution of Fe3+ for Ti4+ as an acceptor center. The position of the iron ion in the ferroelectric phase is found to be similar to the B-site in the paraelectric phase. Partial charge compensation is locally provided by a directly coordinated oxygen vacancy. Using high-resolution synchrotron powder diffraction, it was verified that lead titanate remains tetragonal down to 12 K, exhibiting a c/a-ratio of 1.0721.
English translation
This paper has no Arabic translation yet. Be the first: it takes a few seconds, and the result is stored for every future reader.